The page is under construction and provides only information about standardization documents. You can place an order or request a quotation by emailing us at sales@elot.gr.

ΕΛΟΤ EN ISO 5817 E2

Welding - Fusion-welded joints in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections (ISO 5817:2003, corrected version:2005, including Technical Corrigendum 1:2006)

ΕΛΟΤ EN ISO 5817 E2

Welding - Fusion-welded joints in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections (ISO 5817:2003, corrected version:2005, including Technical Corrigendum 1:2006)

58,00 €

Abstract

ISO 5817:2003 (corrected version:2005) provides quality levels of imperfections in fusion-welded joints (except for beam welding) in all types of steel, nickel, titanium and their alloys. It applies to material thickness above 0,5 mm. It covers fully penetrated butt welds and all fillet welds. The principles of ISO 5817:2003 (corrected version:2005) may also be applied to partial-penetration butt welds.

Info

The standard has been withdrawn

Publication Date

2008-11-12

Withdrawal Date

2014-09-30

Greek Title

Συγκολλήσεις - Ενώσεις με συγκόλληση δια τήξεως σε χάλυβα, νικέλιο, τιτάνιο και τα κραματά τους (εξαιρείται συγκόλληση με δέσμη) - Επίπεδα ποιότητας για ατέλειες (ISO 5817:2003, διορθωμένη έκδοση: 2005, περιλαμβάνει Τεχνική Διόρθωση 1: 2006)

English Title

Welding - Fusion-welded joints in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections (ISO 5817:2003, corrected version:2005, including Technical Corrigendum 1:2006)

Techincal Body

TE 71

Related Documents

ISO 5817 : 2003 - Identical
EN ISO 5817 : 2007 - Identical