ΕΛΟΤ EN 10025-6 Ε2
Hot rolled products of structural steels - Part 6: Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
ΕΛΟΤ EN 10025-6 Ε2
Abstract
This document specifies technical delivery conditions for flat products of high yield strength alloy special steels. The grades and qualities are given in Tables 1 to 3 (chemical composition) and Tables 4 to 6 (mechanical properties) and are supplied in the quenched and tempered condition. The steels specified in this document are applicable to hot-rolled flat products with a minimum nominal thickness of 3 mm and a maximum nominal thickness of 200 mm for grades S460, S500, S550, S620 and S690, a maximum nominal thickness of 125 mm for grades S890 and S960, in steels which, after quenching and tempering, have a specified minimum yield strength of 460 MPa to 960 MPa.
Info
The standard has been withdrawn
Publication Date
2019-08-30
Withdrawal Date
2023-03-30
Greek Title
Προϊόντα θερμής έλασης για χάλυβες κατασκευών - Μέρος 6: Τεχνικοί όροι παράδοσης πλατέων χαλύβδινων προϊόντων με υψηλό όριο διαρροής σε επιβελτιωμένη κατάσταση
English Title
Hot rolled products of structural steels - Part 6: Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
Standard Stage
Techincal Body
TE 49Replaced by
ΕΛΟΤ EN 10025-6+A1:2023Replaces